Once all the other things are in order feeding the filler rod happens naturally.
Tig welding filler rod angle.
This is known as the drag or backhand technique.
5 new welders love to weld with.
Feeding tig filler rods.
Trying to weld 0 035 in.
Just hold onto the wire and stop adding it before your fingers burn.
4 another tig welding mistake to avoid like the plague is using a carbon steel brush to clean aluminum rather that a wire brush made of stainless steel.
There is so much going on with tig welding that it s probably best not to feed the wire for the first few practice beads.
Cagnazzi predominantly uses 0 030 0 045 and 0 063 in.
Stainless steel mild steel copper alloys aluminum alloys nickel alloys titanium alloys.
By the end you will be familiarized with the basics and ready to jump right in and get started on your first tig welding project.
Read about choosing tig welding rods here.
Filler rod is usually added to the puddle of molten metal as the weld progresses.
The arc and molten metal are shielded by an inert gas which protects the electrode and base metal from oxidizing.
Tubing with a 1 16th inch filler 0 063 in is a bad idea because the tubing wall will melt before the filler rod is up to temperature.
The article will cover tig welding gas arcs filler rod and techniques like tig welding aluminum.
In todays video we are going to talk about how i feed filler rod and the importance of being able to do so in the long run.
High performance tig welding filler metal for every application.
If a ball forms on the end of your rod when welding you are doing something wrong.
9 with 045 and 063 being the most common.
It is usually one or more of these things.
312 stainless is also a very good rod choice for welding steel of unknown composition.
Hastelloy w tig welding rod has become extremely expensive.
I know you can probably find many.
Too long an arc too much torch angle not enough amperage for the rod size bad filler rod angle or some combination of all of these things.
Conversely a large filler rod can block the shielding gas and pulls the heat out of the puddle.
With the tig process the heat comes from an electric arc that streams between the electrode in a hand held torch and the metal being welded.
1 16th filler rods fig.
For welding vertical up use a push or forehand technique and tilt the top of the electrode 0 to 15 degrees away from the direction of travel.
For a critical weld you should not just rely on 312 without knowing the metal type you should determine the metal type for any critical weld.
When welding from left to right maintain a 0 to 15 degree angle tilted towards the direction of travel.
This is a basic guideline that no welder should ever forget.